The Xometry app works best with JavaScript enabled!
ResourceseBooks LibraryeBook: Injection Molding Defects (and How to Prevent Them)

eBook: Injection Molding Defects (and How to Prevent Them)

This eBook will go through the types of defects common in injection molding design and how you can prevent them.

an injection molding defect

Injection molding is a manufacturing technique that enables fast and large-scale production of components used in a large variety of industries. Due to the delicacy of this process and its numerous application, there is a wide range of mistakes in the injection molding process that can lead to defects in the injection molded products.

Learn how to prevent common injection molding defects, such as: 

  • Burn Marks
  • Surface Delamination
  • Vacuum Voids
  • Discoloration
  • Warping
  • Flash
  • Sink Marks
  • Weld Lines
  • Jetting
  • Flow Lines
  • Short shots

About Xometry

Xometry offers instant pricing for manufacturing, including precision CNC machining, 3D printing, sheet metal fabrication, injection molding, and urethane casting services. Xometry also provides live engineering support from our team of experts. Upload a 3D CAD file to get an instant quote.

Xometry X Logo
Team Xometry
This article was written by various Xometry contributors. Xometry is a leading resource on manufacturing with CNC machining, sheet metal fabrication, 3D printing, injection molding, urethane casting, and more.

Read more articles by Team Xometry

Support
  • +1-800-983-1959

    support@xometry.com

Mailing Address

© 2026 Xometry, Inc. All Rights Reserved.

Privacy Policy | Terms of Use | Legal